Hard chrome plating typically involves a sulfate-based bath, and the sulfate concentration is an important parameter to monitor. The sulfate concentration in the bath can be determined using the following methods:
1. **Kocour Method**: This is a standard method for measuring sulfate concentration in hard chrome plating baths. It involves adding barium chloride to the solution, which reacts with sulfate ions to form barium sulfate. The precipitate is then filtered, dried, and weighed to determine the sulfate content. 2. **Gravimetric Method**: In this method, a known volume of the plating bath is evaporated to dryness, and the residue is weighed. The sulfate content is then calculated based on the weight of the residue. 3. **Spectrophotometric Method**: This method uses a spectrophotometer to measure the absorbance of a solution containing barium sulfate at a specific wavelength. The absorbance is then used to calculate the sulfate concentration. 4. **Ion Chromatography**: This is a more advanced method that involves separating the sulfate ions from the solution using a chromatographic column and then measuring the concentration of sulfate ions using a conductivity detector. When performing these tests, it's important to follow the specific procedures and standards recommended by the plating bath supplier or industry guidelines to ensure accurate results.Surface finishing is a broad range of industrial processes that alter the surface of a manufactured item to achieve a certain property. Finishing processes may be employed to: improve appearance, adhesion or wettability, solderability, corrosion resistance, tarnish resistance, chemical resistance, wear resistance, hardness, modify electrical conductivity, remove burrs and other surface flaws, and control the surface friction. Contact us - email to vselvaraj@vselvaraj.com
Subscribe to:
Post Comments (Atom)
Innovations in Sustainable Decorative Plating: Insights from the Surface Coating Expo 2025
The Surface Coating Expo 2025 highlighted advancements in sustainable decorative plating, focusing on chrome-free and PAS-free processes. Ke...

-
HEEF 25 is a fluoride-free hard chromium process that offers high current efficiency. It can be adapted for various applications, includin...
-
This blog post provides a comprehensive overview of Hull Cell panels, including their purpose, the equipment needed for interpretation, a...
-
This blog post provides a detailed guide on how to run a Hull Cell, a miniature electroplating cell used to evaluate electroplating solu...
No comments:
Post a Comment
Note: Only a member of this blog may post a comment.