New Developments in EN Corrosion Protection

For your requirement of electroless nickel plating chemiclas contact us at 9843019701 or email to info@essess.trading

About This Webinar
Electroless deposition of nickel-phosphorus alloy (Ni-P) coatings is very popular in many industrial applications due to its unique properties such as corrosion resistance, wear resistance, non-magnetism, improved micro-hardness and coating thickness uniformity.

Due to its amorphous character and passivity, the corrosion resistance of these coatings, especially of high-P EN, is excellent and in many environments even better than that of pure nickel or chromium alloys.

Global regulations have restricted the use of heavy metals as stabilizers and brighteners in electroless nickel processes, so today's new generation of high-P EN processes use metal-free or toxic heavy metal-free stabilizers. These are not only environmentally friendly alternatives, but also offer improved process parameters and coating properties in terms of deposition rate, P content, internal stresses, tribological properties and corrosion resistance.

With a strong commitment to sustainability, Atotech continues to pioneer the conversion of the coating industry to environmentally sound processes and currently offers a complete range of electroless nickel processes that meet and exceed all national environmental regulations. Therefore, we are pleased to present in this webinar our latest development of ELV, ROHS and WEEE compliant, highly corrosion resistant EN processes meeting the ever-increasing industrial requirements.
Agenda
  • Corrosion of EN coatings: Mechanism and test methods
  • Factors that mainly influence the corrosion protection of EN coatings
  • Corrosion performance of EN processes
  • New highly corrosion resistant processes from Atotech

Advertisement

Wednesday, November 4, 2020

Zinc & Zinc Alloy Plating

Topic: Zinc & Zinc Alloy Plating

Speaker: Mr. T.K. Mohan

General Manager(W) Consolidated Metal Finishing Pvt. Ltd.


Contact us for your requirement for Zinc and Zinc alloy Plating chemicals 

ESS ESS TRADING 23 Vetrilaikara Street, Peelamedu coimbatore -641004 

Email: info@essess.trading   Mobile: 9843019701

கோயம்புத்தூர் மண்ணில் பிறந்தோம் நாங்க

கோயம்புத்தூர் மண்ணில் பிறந்தோம் நாங்க மின்பூச்சு தொழிலில் வாழ்க்கை அமைத்தோம் எலக்ட்ரோப்பிளேட்டர்ஸ் சங்கம் எங்கள் வீடு எக்செல் லேபரட்டரீஸ் ...