Hell is a testing tool, or a miniature electroplating cell, in which an electroplating solution is evaluated across the range of operating conditions. This video will show you how to run a hull cell.

Please see the following videos one by one..

Hull Cell Description video 1

Interpreting Hull Cell Panels video 2

Interpreting Hull Cell Panels video 3

Nickel plating baths should be evaluated using either brass hull cell panels or the standard zinc coated, steel hull cell panels used to evaluate many other plating baths. In this video we discuss the proper way to interpret nickel plated hull cell panels.

Interpreting Zinc Plated Hull Cell Panels video 4

Zinc plating baths of all types, alkaline or acid demonstrate similar characteristics when evaluated using a hull cell. In this video we explain how to properly interpret zinc plated hull cell panels.

--------------------------------------------------------------------